NB109 vs phosphor bronze: terminals that carry current

Choose NB109 when the terminal carries current: at 40 % IACS it conducts about three times better than phosphor bronze, which lowers temperature rise, and it holds contact force better at elevated temperature. Choose phosphor bronze when the current is small and the spring needs more than about 590 MPa.

Side-by-side data

NB109C5191C5210
UNSC19025C51900C52100
EquivalentsJASO JC400EN CuSn6 / CW452K; JIS C5191; GB QSn6.5-0.1EN CuSn8 / CW453K; JIS C5210; GB QSn8-0.3
Composition %Ni 1.0, Sn 0.90, P 0.05Sn 5.5 – 7.0, P 0.03 – 0.35, Cu + Sn + P ≥ 99.5Sn 7.0 – 9.0, P 0.03 – 0.35, Cu + Sn + P ≥ 99.7
Conductivity %IACS4013 – 15≈ 12
Tensile strength MPa440 – 590315 – 685470 – 885
Tempers1/2H, H, EHO, 1/4H, 1/2H, H, EH1/2H, H, EH, SH, ESH
Elastic modulus130 GPa110 GPa110 GPa
Density8.9 g/cm³8.83 g/cm³8.80 g/cm³

Tensile strength is the range across supplied tempers. Full composition, tempers and physical properties are on each grade page.

Choose NB109 when

Choose phosphor bronze when

Notes

NB109 is a copper-nickel-tin-phosphorus alloy registered as UNS C19025. Its lower strength ceiling is the trade-off for the higher conductivity.

Questions buyers ask

Does switching from phosphor bronze to NB109 reduce temperature rise?

For the same geometry, yes: bulk resistance falls by roughly two thirds. The measured result depends on the contact interface and plating, so confirm it with a temperature-rise test.

Need a recommendation for a specific part?

Tell us the part function, strip thickness and performance targets. We reply within one working day, and sample coils are available for comparative trials.